Get in Touch with Saiweiglass
A cold mirror is a specialized dielectric reflector that bounces visible light toward a target while letting infrared heat pass straight through its glass substrate. As Robert Cabrera reports in Laser Focus World, a 45° cold mirror reflects about 95% of white light and transmits an average of 90% of infrared energy above 750 nm. Folding the beam keeps destructive heat off sensors, film gates, and micro-displays.
Depending on the substrate chemistry and type of coatings, transmitted thermal energy can clear the housing safely. Low-expansion borosilicate mirror blanks and synthetic fused silica can withstand high temperature gradients beyond which ordinary float glass will crack. Combining the blank with a backside anti-reflective coating suppresses exit-face ghosting in downstream imaging lenses.
Key Engineering Takeaways
- Multi-layer oxide stacks separate visible illumination from near-infrared heat through thin film interference rather than bulk dye absorption.
- Tilting a normal-incidence coating to 45 degrees blue-shifts its transition edge and splits S and P polarized beams.
- Silicate substrates pass near infrared radiation up to 2000 nm, but absorb mid-infrared energy (2500 nm and higher) and heat the mirror substrate.
- Standard 1 in, 2 in, and 4 in catalog optics ship from inventory, while custom enclosures use CNC-machined borosilicate, aluminosilicate, low-iron, or soda-lime blanks.
What Is a Cold Mirror and How Does Dielectric Heat Separation Work?

Multi-layer stacks reflect visible light from a front thin-film surface while passing near-infrared heat through the transparent rear face. Commercial 45° designs reflect above 90% across 425–650 nm and transmit over 85% from 800 to 1200 nm, as listed in RP Photonics supplier specifications. Use an absorptive filter only when housing geometry blocks a rear heat dump.
A practical analogy is to consider the coating as more of a wavelength-selective sieve than a dark sponge. As explained in the thin-film optics notes by the University of Arizona, quarter-wave metal oxide films alternating between high- and low-index refractive layers sit on the front glass face. Reflected visible waves are in-phase and add constructively, and the longer infrared waves cancel in reflection and transmit through the blank.
Every watt follows optical energy conservation in reflection, transmission, and bulk absorption. Our reference on how light interacts with optical glass illustrates this principle at bare and coated interfaces. Unlike dichroic isolated-line optical filters for single laser wavelengths, a broadband multi-layer dielectric stack covers the visible spectrum.
Reflections at the exit face are critical in sensitive optical components. According to SW Glass optical transmittance benchmarks, each untreated glass face in air reflects 4.0% to 4.2% of normal-incidence light. If there is no rear anti-reflective coating, that exit reflection creates a ghost image and reflects NIR back toward the target.
Cold Mirror vs. Hot Mirror: Beam-Folding or Inline IR Rejection?

Pick a beam-folding cold mirror if your housing has space behind the mount to place an infrared heat sink away from the lamp. Only pick an inline hot mirror if a straight optical design can’t fold by 90 degrees and the lamp compartment vents reflected heat.
Folding Cold Mirror
- Turns visible white light into a cool orthogonal arm.
- Passes near-infrared heat straight into a rear absorber.
- Protects lamp pinch seals from reflected thermal energy.
- Requires a right-angle bend in the optical housing.
Inline Hot Mirror
- Transmits visible light straight down an existing lens tube.
- Reflects 90%–95% of 750–1200 nm heat back upstream, per Laser Focus World.
- Fits retrofits where mechanical folding is impossible.
- Can overheat bulbs if placed in front of a lamp without cooling.
Broadband first-surface mirrors with protected aluminum films reflect both visible and near-infrared radiation down the same path, as noted in MIT’s optical reflector reference. Infrared-absorbing glass panes soak up heat in the bulk material, altering color neutrality and cracking under focused beams. Hot and cold mirrors separate bands by interference.
| Optic Type | Typical AOI | Visible Action | NIR / Heat Action | Primary Optical Fit |
|---|---|---|---|---|
| Visible Cold Mirror (Folding) | 45° | Reflects ~95% white light | Transmits ~90% above 750 nm | Tungsten projectors and folded lamp engines |
| Normal-Incidence Cold Mirror | 0° | Reflects >90% back on axis | Transmits >85% straight behind | Normal-incidence cavity and sensor return paths |
| Standard Dielectric Hot Mirror | 0° | Transmits >85% inline | Reflects 90%–95% (750–1200 nm) | Xenon or metal-halide inline lens tubes |
| Beam-Splitting Hot Mirror | 45° | Transmits >85% straight ahead | Reflects >90% NIR to side sink | Inline visible channels needing side IR exhaust |
| Extended Hot Mirror | 0° | Transmits visible spectrum | Blocks infrared out to 1600 nm | Acrylic fiber illuminators absorptive above 1000 nm |
| Narrowband UV Cold Mirror | 45° | Reflects >99% at 365 nm; passes 90% VIS | Transmits 90% average infrared | Mercury-line adhesive curing and exposure |
| UV-Pass Hot Mirror | 0° | Passes 80% UV down to 250 nm | Reflects ~75% of 800–1100 nm heat | Broadband 220–440 nm ink curing on fused silica |
| IR-Absorbing Filter Glass | 0°–45° | Moderate visible pass; non-neutral tint | Absorbs IR in bulk; fails under focus | Wide-angle operator displays needing angle stability |
| Protected Aluminum Mirror | 0°–45° | Reflects ~90% visible light | Reflects NIR down the same path | Low-heat routing where IR separation is unnecessary |
How do hot mirrors work?
An optical hot mirror uses a dielectric thin-film stack to transmit visible light inline while reflecting 90% to 95% of near-infrared energy between 750 and 1200 nm. Although optical hot mirrors and automotive defrost mirrors share a name during general web searches, they share no similarities. The oxide interference layers of the optical hot mirror reject unwanted heat passively.
Lamp spectrum dictates where that reflected heat travels. In solar-simulator experiments published on NIH PubMed Central, researchers pair a short-pass hot mirror blocking IR light above 700 nm with a long-pass cold filter isolating wavelengths below 700 nm. Because tungsten-halogen bulbs radiate heavily beyond 1600 nm, placing a normal-incidence hot mirror directly against an uncooled bulb overheats the filament.
Spectral Specifications: Cut-Off Wavelength, Passband Ripple, and Backside AR

Specify four core parameters on any spectral drawing: visible average reflectance (≥90%–95% over 400–690 nm), NIR passband transmission (≥85%–90% over 750–1200 nm), 50% cut-off wavelength tolerance, and rear anti-reflective reflectance below 1% across 700–1150 nm. Pair those bands with the cut-off wavelength tolerance and exit-face anti-reflective coating reflectance so color balance, heat rejection, and sensor ghosting stay controlled.
The cut-off wavelength defines the midpoint transition from visible reflection to infrared transmission. A catalog dichroic filter typically specifies bands such as 420–630 nm reflectance paired with 750–1200 nm passband transmission, holding transition tolerances within ±15 nm to ±25 nm across commercial series. Within the transmission passband, thin-film interference results in ripples known as passband ripple, and local troughs of transmission fall below the band average.
Backside coatings protect contrast whenever cameras or projection lenses sit downstream. Multi-layer anti-reflective films raise visible glass transmission from 89%–90% to 95%–98%, while high-performance catalogs hold exit-face reflectance below 1% across 700–1150 nm. Our engineering note on exit-face AR index-matching films details rear-surface reflection control. Guaranteed catalog reflectance and transmission bands hold strictly within the clear aperture and shaded wavelength regions.
What limits the performance of a cold mirror?
Four physical limits in the performance of a cold mirror are incidence-angle shift, blue and red edge roll-off, oblique polarization splitting, and silicate glass absorption above 2500 nm. Dr. Rüdiger Paschotta, in the RP Photonics Encyclopedia, notes that sustaining high reflectivity across the entire visible spectrum is challenging for a dielectric mirror, leading to losses at the blue and red extremes.
Converging illumination cones strike the coated surface simultaneously across a wide spread of angles. Rays at 35° and rays at 55° experience different optical path lengths inside the stack, smearing the 700 nm transition edge. Collimating the lamp output before the fold mirror preserves spectral purity and even field color.
Angle of Incidence (0° vs. 45° AOI) and Polarization Splitting

Mount every dielectric reflector at its rated angle of incidence, because 0° and 45° coatings aren’t interchangeable. At a 45° angle of incidence, size the mirror blank to at least 1.414x the circular beam diameter along the tilt axis, so the projected ellipse clears the coated aperture.
For an interference stack, the reflection band shifts toward shorter wavelengths as the oblique refraction angle increases. Per the RP Photonics Encyclopedia, dielectric reflection spectra are tuned for a specific angle such as normal incidence or 45°, degrading sharply at off-design angles. Deep-red visible wavelength leakage through the back surface of the film results in a cyan-tinted white reflection.
Oblique reflection separates linear polarization components. The S-polarization oscillates in the direction parallel to the axis of the mirror tilt. The P-polarization oscillates in the direction perpendicular to the axis of the mirror tilt. In liquid crystal light engines or polarized laser trains, S-polarized light holds a wider reflection band, thus splitting the cut-off edge between the two states.
Precise mechanical sizing accounts for elliptical footprint projection on tilted mounts:
- Divide the diameter of the circular beam in question by cos(45°) to find the required tilt axis clear aperture, which is equal to beam diameter × 1.414.
- A collimated 20 mm circular beam striking a tilted fold plate projects a 20 mm × 28.28 mm ellipse, clipping inside a Ø1 in (25.4 mm) round ring.
- Standard kinematic holders pair Ø1 in, Ø2 in, and rectangular 25 mm × 36 mm plates with filter cubes so rectangular optics clear circular beams cleanly.
| Design Parameter | 0° AOI Configuration | 45° AOI Configuration |
|---|---|---|
| Reflected Visible Path | 180° return along input axis | Orthogonal fold away from heat axis |
| S / P Polarization Behavior | Identical s and p spectral curves | Split s and p transition edges; specify polarization |
| Footprint Along Tilt Axis | 1.00× circular beam diameter | 1.414× circular beam diameter (25 × 36 mm or Ø2 in) |
| Result if Cross-Substituted | 45° part at 0° shifts cut-off redward, reflecting short-wave NIR and leaking violet | 0° part at 45° shifts cut-off blueward, leaking deep-red visible light |
3-Band Heat-Split Budget: Worked Thermal Example for Lamp and Laser Optics

On an assumed 100 W broadband lamp (25 W visible, 65 W near-infrared, and 10 W mid-infrared), a dielectric cold mirror cuts folded target load from 90.00 W on aluminum down to 30.25 W. It dumps 61.75 W behind the mount while absorbing 8.00 W of mid-infrared in the glass.
3-Band Heat-Split Budget
This optical heat-split model calculates reflected visible power, transmitted near-infrared load, and absorbed or dumped heat across candidate mirrors under stated lamp assumptions.
Assumed inputs: Take a steady-state 100 W collimated source split into 25 W visible (400–690 nm), 65 W near-infrared (750–2000 nm), and 10 W mid-infrared (above 2500 nm). Model the cold mirror at Rvis = 0.95, Rnir = 0.10, and Tnir = 0.90 per Laser Focus World, with 80% bulk glass absorption above 2500 nm. Compare that against protected aluminum at 90% reflectance across all three bands.
| Power Channel & Formula | Dielectric Cold Mirror | Protected Aluminum Mirror |
|---|---|---|
| 1. Folded Visible (25 W × Rvis) | 25 W × 0.95 = 23.75 W | 25 W × 0.90 = 22.50 W |
| 2. Folded Residual NIR (65 W × Rnir) | 65 W × 0.10 = 6.50 W | 65 W × 0.90 = 58.50 W |
| 3. Folded Mid-IR (10 W × Rmir) | 10 W × 0.00 = 0.00 W | 10 W × 0.90 = 9.00 W |
| Total Power Reaching Target | 23.75 + 6.50 + 0.00 = 30.25 W | 22.50 + 58.50 + 9.00 = 90.00 W |
| Rear Exhaust Power (VIS + NIR + Mid-IR) | 1.25 + 58.50 + 2.00 = 61.75 W | 0.00 W (opaque metal film) |
| Power Absorbed in Mirror | 8.00 W (mid-IR glass absorption) | 10.00 W (metal film absorption) |
Assuming the input values are correct, replacing aluminum with a dielectric reflector will strip 59.75 W of heat from the folded beam while adding 1.25 W of extra visible light. That steady-state condition compares optical routing rather than air convection through the enclosure, so further testing with thermocouples on the lamp housing is required.
Kilowatt laser systems generate noticeable mirror heating even when near-infrared transparency reaches 97%. Under a 1.5 kW, 810 nm fiber-coupled diode laser, optical combiner tests show a 97% transmitting splitter still experiences roughly 50 W of heating. Polymer lightguides also need protection because Laser Focus World measurements show acrylic fibers absorb below 375 nm and above 1000 nm, turning opaque above 1620 nm.
Selecting IR-Transmitting Substrates: Soda-Lime, Borosilicate, and Fused Silica

Choose borosilicate 3.3 (3.25 × 10⁻⁶ /K, rated up to 450 °C) for halogen projectors, or synthetic fused silica (0.55 × 10⁻⁶ /K, bare substrate rated to 950–1,050 °C; dielectric stacks up to 600 °C) for kilowatt laser systems and UV optics. Limit annealed soda-lime glass (8.6-9.0 × 10⁻⁶ /K) to low-power benches below its 40-50 °C quench survival limit.
Unlike front-surface metal mirrors, where rays don’t enter the blank, a cold mirror passes infrared energy right through its substrate. At room temperature, silicate glass conducts heat at the rate of 0.80 to 1.38 W/(m·K). Soda-lime thermal expansion runs nearly 3 times higher per degree C than borosilicate. Rapid cooling at the edges of high-expansion float glass, after the lamps shut off, can cause thermal stress and cracking.
Published data in the SCHOTT BOROFLOAT datasheet lists a 2.22 g/cm³ density, 63 GPa Young’s modulus, and refractive index nd = 1.472 alongside 160 °C annealed thermal-shock resistance. As described in Florida State University’s optics primer, synthetic fused silica adds broadband UV-to-IR transmission (185 nm to 3,500 nm) and polishes to tight laser-mirror tolerances. Borosilicate and soda-lime transmittance drops sharply above 2500–2700 nm into bulk mid-infrared absorption, meaning tungsten-halogen lamps still heat the glass blank itself.
| Substrate Material | Linear CTE (0–300 °C) | 3 mm Cold Quench Survival | Max Continuous Service | Refractive Index (nd) & Window |
|---|---|---|---|---|
| Soda-Lime Float Glass | 8.6 – 9.0 × 10⁻⁶ /K | 40 – 50 °C (Annealed) | Below 200 °C | 1.520; blocks deep UV <310 nm |
| Borosilicate 3.3 (Borofloat) | 3.25 – 3.30 × 10⁻⁶ /K | 160 °C (Annealed) / 260 °C (Tempered) | Up to 450 °C | 1.472; high VIS and NIR clarity |
| Synthetic Fused Silica (SiO₂) | 0.55 × 10⁻⁶ /K | > 800 °C | Bare glass 950–1,050 °C; coated stack ≤600 °C | 1.458; 185 nm UV to 3,500 nm IR |
How much heat can a cold mirror withstand?
Coated all-dielectric cold mirrors on low-expansion substrates can withstand continuous temperatures up to 450 °C on borosilicate per SCHOTT BOROFLOAT data and up to 600 °C on hard-coated specialty blanks in RP Photonics supplier specifications. Under these conditions, surface dust and localized thermal gradients may cause the glass to fail well below the uniform limit of the oven.
Dust on the front of the dielectric coating absorbs heat from the lamps and creates micro hot spots. Sealing the lamp housings with filtered cooling air prevents localized film crazing and substrate cracking.
Dielectric Coating Stacks, UV Cold Mirrors, and ISO 9211 Durability

Specify ion-assisted deposition (IAD) hard oxide stacks for humid housings or arc-lamp cycling, and reference ISO 9211-2:2024 for optical properties. Pair it with ISO 9211-3:2024 and ISO 9211-4:2022 for environmental durability, abrasion, adhesion, and water resistance, since conventional electron-beam chambers heat substrates near 300 °C.
“By bombarding the films with high-energy ions during the deposition process, IAD increases the refractive index of the evaporated films and reduces the porosity of the film. This greatly increases the stability and durability of the coating.”
Each added oxide layer increases mechanical film stress, capping total layer count and blocking bandwidth. Dense IAD films keep moisture out of microscopic pores so spectral cut-offs stay stable in outdoor housings. Standard quality callouts combine ISO 9211-3:2024, ISO 9211-4:2022, and MIL-C-48497A snap-tape, humidity, and moderate abrasion tests so coatings do not peel or degrade during cleaning.
What is a UV cold mirror?
A UV cold mirror is an ultraviolet-reflecting interference optic that directs curing or exposure wavelengths below 400 nm onto a target while transmitting visible and infrared heat. As Laser Focus World notes, a 20-layer stack provides over 99% reflection at the 365 nm mercury line with 90% average visible and infrared transmission.
Catalog ultraviolet reflectors also cover wider bands such as 325–475 nm reflection with >85% transmission from 600 to 1200 nm. Semiconductor photolithography and photopolymerization lines for inks or adhesives rely on this heat control, as outlined by RP Photonics. When broadband inks require 220–440 nm curing where low-index UV materials demand high layer counts, a fused silica UV-pass hot mirror passing 80% down to 250 nm can lower filter cost.
Optical System Applications and Rear Heat-Sink Engineering

Every cold-mirror enclosure requires a blackened, finned rear heat sink, or vented exhaust duct, behind the substrate.
Combine that absorber with compliant spring clips, as bare aluminum walls bounce infrared light right back into the optical system.
Thermal drift degrades focus in precision optics before glass fractures. In a concentrator lens experiment described in the article posted at NIH PubMed Central, a 20 °C warm-up expanded the spot size by 30% on the top band and by as much as 60% on the middle band. In vehicle cockpits described by U.S. Patent US11586039B2, a cold mirror is used as the head-up display fold optic. It directs reverse solar heat away from the panel behind automotive display glass. Analytical labs have verified UV-to-IR spectra from 175 nm to 16,000 nm, as described by EAG Laboratories.
| Optical System Application | Target Spectral Role | Recommended Substrate | Rear Thermal & Mount Design |
|---|---|---|---|
| 1. Tungsten-Halogen Projectors | Fold white light; pass >750 nm IR | Borosilicate 3.3 | Forced-air exhaust duct behind fold mount |
| 2. 4000 W Metal-Halide Luminaires | Fold visible; dump intense NIR band | Borosilicate 3.3 or Fused Silica | Spring-clip expansion gap + finned black plate |
| 3. Automotive Head-Up Displays (HUD) | Fold display image; pass solar IR load | Borosilicate 3.3 (custom contour) | Blackened solar heat trap below mirror cavity |
| 4. Acrylic Fiber-Optic Illuminators | Fold visible; strip <375 nm & >1000 nm | Borosilicate 3.3 | Combine fold mirror with UV/extended-IR blocking |
| 5. Xenon Solar Simulators (300–1800 nm) | 700 nm dichroic sub-cell test split | Fused Silica or Borosilicate 3.3 | Exit-face AR coating to eliminate CCD ghosting |
| 6. 365 nm Mercury UV Curing Lines | Reflect 365 nm UV; pass VIS & IR heat | Synthetic Fused Silica | Water- or air-cooled rear absorber behind lamp |
| 7. Semiconductor Photolithography | Reflect 325–475 nm exposure band | Synthetic Fused Silica | Low-stress 3-point kinematic mount + rear AR |
| 8. Kilowatt 810 nm Laser Combiners | Fold visible; 97% pass at 810 nm | Synthetic Fused Silica (laser polished) | Active cooling for ~50 W residual thermal load |
| 9. Low-Power Benchtop Inspection | Reflect 420–630 nm; pass NIR | Soda-Lime Float (1.0 mm stock) | Standard Ø1 in or 25 × 36 mm filter cube mount |
In machine-vision light engines and projection systems, don’t clamp metal retaining rings directly to bare glass corners. A compliant pad gap allows the blank to expand and contract freely under lamp heat.
Stock vs. Custom Cold Mirror Pricing, Tolerances, and RFQ Checklist

Buyers source cold mirrors through three channels: single-unit stock catalog optics (1 in, 2 in, and 4 in round or square, plus 25 × 36 mm plates), custom-diced pre-coated stock sheets, or full custom coating batches. Standard stock sizes ship from warehouse inventory, whereas non-standard cut-offs, drilled mounting holes, or laser-threshold stacks require chamber batch quoting. Published catalog prices for 1 mm soda-lime visible cold mirrors at 45° AOI run $41.00 for Ø1 in, $77.22 for Ø2 in, and $93.43 for 25 mm × 36 mm plates, whereas custom substrates or stacks require drawing-based RFQ pricing.
Surface tolerances drive unit price far more than glass thickness. Non-imaging illumination reflectors perform cleanly with commercial 4–6λ flatness and 60-40 or 80-50 scratch-dig surface quality under ISO 10110-7:2017. Specifying sub-wavelength imaging figure on a lamp fold plate forces pitch polishing and interferometric testing without adding screen lumens.
Speeding up OEM procurement hinges on lining up drawing stages with supplier capabilities. Thin-film coating houses deposit custom dielectric stacks, while SW Glass CNC-machines borosilicate 3.3, aluminosilicate, low-iron, and soda-lime blanks to ±0.05 mm accuracy with 220–400 grit diamond-polished C-edges or chamfers. Our Dongguan plant is able to provide CNC prototypes with spectrophotometer logs and AG, AR, AF, and ITO treatments in 7-10 days through our precision optical substrate fabrication.
| RFQ Field | Recommended Starting Spec | Why It Prevents Re-Quoting |
|---|---|---|
| Design AOI & Polarization | 0° or 45° AOI; state unpolarized, s, or p | Prevents cyan color shift and s/p edge mismatch |
| Reflection & Pass Bands | State target visible Ravg and NIR Tavg intervals | Fixes visible throughput and heat rejection over clear aperture |
| Rear Surface Treatment | Uncoated for lamp folding; NIR AR film for imaging | Suppresses exit-face Fresnel ghosting on downstream sensors |
| Substrate Family | Borosilicate 3.3 (general) or Fused Silica (UV / high-power laser) | Matches thermal shock survival to lamp irradiance |
| Aperture & Edge Profile | Account for elliptical tilt footprint; diamond C-edge or chamfer | Clears angled beam and removes edge micro-fissures |
| Surface Quality & Durability | 60-40 or 80-50 (ISO 10110-7:2017); IAD per ISO 9211-3:2024 | Avoids cosmetic over-polishing while locking humidity resistance |
| Coated-Face Marking | Edge arrow or bevel indicator on dielectric front side | Stops assembly crews from installing the blank backward |
Frequently Asked Questions
What are the differences between a hot mirror and a cold mirror?
A cold mirror reflects visible wavelengths and transmits infrared heat through its rear substrate and typically folds the cooler visible beam into an orthogonal arm. A hot mirror works in reverse by passing visible light inline and reflecting infrared energy upstream. Pick a folding reflector where space permits, to trap heat away from the lamp.
Which side of a cold mirror faces the light source?
Orienting the dielectric-coated front surface toward the incoming light source works the same as orienting a front-surface reflector. Optical fabricators mark that coated surface with a bevel or edge pencil arrow so the oxide film isn’t disturbed. Backward mounting of the blank sends visible light through the glass twice, creates front-surface ghosting, and builds up bulk heat in the reflector.
Can I use a 0-degree cold mirror at a 45-degree angle?
No, a cold mirror coated for normal incidence shouldn’t be installed at an oblique fold angle in color-critical or polarized optical systems. Tilting a normal-incidence interference stack reduces the effective optical path, shifts the cutoff blueward into red light, and splits the polarization bands. Deep-red wavelengths leak out the rear face and tint the reflected beam cyan.
Will a mirror break if it gets too cold or thermally shocked?
Abrupt temperature differentials rather than steady cold conditions fracture optical blanks. Choose low-expansion borosilicate 3.3 or synthetic fused silica rather than annealed float glass under rapid lamp cycling.
How do you clean a dielectric cold mirror safely?
Blow dust and grit off with filtered dry air or nitrogen, and then gently wipe with optical lens tissue moistened with reagent grade isopropyl alcohol or acetone.
Does a standard cold mirror reflect ultraviolet light?
No, standard visible cold mirrors are designed for the visible spectrum rather than ultraviolet radiation. Curing adhesives at 365 nm or exposing photoresists requires a dedicated UV cold mirror deposited on synthetic fused silica with a tuned ultraviolet stack. Soda-lime blanks block deep UV below 310 nm, while visible oxide stacks pass or absorb near-UV energy.
Need Custom-Machined Optical Glass Substrates or AR Surface Treatments?
Provide your dimensional CAD drawing, substrate grade (borosilicate 3.3, aluminosilicate, low-iron, or soda-lime), edge chamfer, and surface coating specs to SW Glass.
Reviewed by the SW Glass technical team.
References & Sources
- Coatings separate heat from light (Robert Cabrera) Laser Focus World
- Cold Mirrors, Heat Control Filters & Dielectric Reflectors (Dr. Rüdiger Paschotta, DOI 10.61835/h71) RP Photonics Encyclopedia
- Thin-Film Multilayer Cold Mirror Optics Lecture Notes College of Optical Sciences, University of Arizona
- Optical Reflector Coatings Technical Reference Massachusetts Institute of Technology (MIT DSpace)
- Indoor Experimental Assessment of Fresnel Lenses with Dichroic Hot and Cold Mirrors (PMC5755248) U.S. National Library of Medicine / National Institutes of Health
- SCHOTT BOROFLOAT Technical Data Sheet University of Chicago Physical Sciences Division Archive
- Introduction to Mirrors and Fused Silica Substrates Molecular Expressions, Florida State University
- ICS 37.020 Optical Equipment Catalogue (ISO 9211-2:2024, ISO 9211-3:2024, ISO 9211-4:2022, ISO 10110-7:2017) International Organization for Standardization (ISO)
- U.S. Patent US11586039B2: Vehicle Projection Assembly with Multilayer Cold Mirror Google Patents / U.S. Patent and Trademark Office
- Application Note: Physical and Optical Properties of Glass Eurofins EAG Laboratories